ION-NOSTAT Comfort I.2

Cleanroom garment fabric

The cleanroom fabric ION-NOSTAT Comfort I.2 is based on microfibres and hence excels in good wearing comfort characteristics. The very high breathability combined with a very pleasant soft touch are the corresponding uniquely selling points.

Also to be pointed out are the particle retention capacity and the good to very good antistatic characteristics of ION-NOSTAT Comfort I.2. Although this cleanroom fabric is based on microfibres, the values for abrasion resistance and roughening disposition can be classified from average to adequate.

Fabric properties Important properties at a glance

  • LAir Permeability
  • TWearing comfort
  • PParticle retention capacity
  • EElectrostatic behaviour
  • AAbrasion resistance

Available colors


Product recommen­dation based on cleanroom classes

Air cleanliness class EN ISO 14644-1
particulate monitored areas

123456789low dust

Hygiene zones according to GMP
microbiological monitored areas

ABCDE

Technical data

(3) Fabric 98% polyester, 2% carbon
(3) Distances of the electrically conductive yarn in warp and weft at 5 mm intervals
(3) Weave type 2/1 twill
(3) Conductive material/yarn carbon fibre, sheath construction
(3) Mass per unit area approx. 105 g/m2
(1) Air permeability according to DIN EN ISO 9237:1999-12 at 200 Pa 38.7 L/(dm2 x min)
(2) Water-vapour resistance DIN EN ISO 11092:2014-12, Ret = m2 Pa/W Ret 1.95 (very good)
(1) Particle retention capacity (VDI 3926)against airborne particles
Test duration: 60 minutes
Raw gas concentration: 25 mg/m3
≥ 0.5 μm approx. 96%
≥ 5.0 μm approx. 97%
(1) Triboelectric behaviouraccording to DIN EN 1149-3 method 1 (ITV-TEV method) good
(3) Surface resistivity according to DIN EN 1149-1:2006-09Protective clothing - Electrostatic properties - Part 1: Test method 106 - 108 Ohm
(1) Abrasion resistance referring to DIN EN ISO 12947-4Martindale method - assessment of appearance change medium - sufficient

The above-mentioned data are the results of investigations carried out by neutral textile research institutes and our suppliers to the best of their knowledge. They are not specifications but typical values at the time of publication.

All statements are without guarantee and changes are possible without prior notice.

Due to different test methods depending on the respective manufacturers and test institutes, the majority of the stated values cannot be compared one-to-one with those of other cleanroom fabrics.

(1) Values determined by the Institute for Textile and Process Engineering Denkendorf
In May 2017 the ITV Denkendorf merged into the public trust DITF Denkendorf. 
(2) Values determined by the Hohenstein Textile Testing Institute (HTTI)
(3) Manufacturer information

Test results after 50 decontamination cycles.

Synthetic fabrics can shrink up to 3% during the decontamination process.
If such a textile is additionally autoclaved, the shrinkage has an even stronger optical effect due to the associated formation of wrinkles.

Version 09/2019