Skip to main content

ION-NOSTAT LS LIGHT 125.2

Cleanroom garment fabric

The cleanroom fabric ION-NOSTAT LS Light 125.2 is a compromise between the typical cleanroom fabric requirements in view of filtration efficiency, abrasion resistance and own particle emission, as well as the highest possible wearing comfort, breathability and pleasant feel (haptics).

The values for conductivity are satisfactory. The filtration efficiency and the abrasion resistance (roughening disposition) conform to the typical requirements of the actual application area, so the requirements of an ISO 8/ISO 9 area (ISO 14644-1) or hygiene zones D and E (Regulation (EU) for GMP).

Fabric properties Important properties at a glance

  • LAir Permeability
  • TWearing comfort
  • PParticle retention capacity
  • EElectrostatic behaviour
  • AAbrasion resistance

Available colors


Product recommen­dation based on cleanroom classes

Air cleanliness class EN ISO 14644-1
particulate monitored areas

123456789low dust

Hygiene zones according to GMP
microbiological monitored areas

ABCDE

Technical data

(3) Fabric 98% polyester, 2% carbon
(3) Distances of the electrically conductive yarn in warp and weft at 8 mm intervals
(3) Weave type 2/1 twill
(3) Conductive material/yarn carbon fibre, sheath construction
(3) Mass per unit area approx. 123 g/m2
(1) Air permeability according to DIN EN ISO 9237:1999-12 at 200 Pa 212 L/(dm2 x min)
(2) Water-vapour resistance DIN EN ISO 11092:2014-12, Ret = m2 Pa/W Ret 2.05 (very good)
(1) Particle retention capacity (VDI 3926)against airborne particles
Test duration: 60 minutes
Raw gas concentration: 25 mg/m3
≥ 0.5 μm approx. 67%
≥ 5.0 μm approx. 76%
(1) Triboelectric behaviouraccording to DIN EN 1149-3 method 1 (ITV-TEV method) good
(3) Surface resistivityaccording to DIN EN 1149-1:2006-09Protective clothing - Electrostatic properties - Part 1: Test method 106 - 109 Ohm
(1) Abrasion resistancereferring to DIN EN ISO 12947-4Martindale method - assessment of appearance change sufficient

The above-mentioned data are the results of investigations carried out by neutral textile research institutes and our suppliers to the best of their knowledge. They are not specifications but typical values at the time of publication.

All statements are without guarantee and changes are possible without prior notice.

Due to different test methods depending on the respective manufacturers and test institutes, the majority of the stated values cannot be compared one-to-one with those of other cleanroom fabrics.

(1) Values determined by the Institute for Textile and Process Engineering Denkendorf
In May 2017 the ITV Denkendorf merged into the public trust DITF Denkendorf. 
(2) Values determined by the Hohenstein Textile Testing Institute (HTTI)
(3) Manufacturer information

Test results after 50 decontamination cycles.

Synthetic fabrics can shrink up to 3% during the decontamination process.
If such a textile is additionally autoclaved, the shrinkage has an even stronger optical effect due to the associated formation of wrinkles.